Published Aug. 8, 2017, 4:53 p.m.
<p>The enamel surface is matt in all the areas where the enamel has been ground back. In the places where the enamel is not matt this means I could probably do with adding some more enamel to increase the surface height in these sections.</p> <p>Here you can see the enamel near to the outside border has not been ground back, in this case this is due to the border ring being too high and I haven't ground enough of it away yet.</p>
This photo is found in the following galleries:
Cloisonné Amazon Frog |